Feb 01, 2013 For quenching, the melt was rapidly poured into a water bath at room temperature. The quenched glass was then dried at 110 C for 24 h in air and was ground in a disk type ball mill. After milling, the glass powder was pressed into cylindrical shape having a diameter of 10 mm and length of 30 mm without using any binder